Smelting Process with Reduction and Sulfur-Fixation for Lead-bearing Solid Wastes

Lu-lu GUO,Yong-ming CHEN,Jing HE,Yue-jun WANG,Long-gang YE,Chao-bo TANG,Sheng-hai YANG
DOI: https://doi.org/10.3969/j.issn.0253-6099.2017.05.018
2017-01-01
Abstract:In order to effectively recycle and utilize the lead-bearing wastes including zinc plant residues and spent lead-acid battery paste, a new smelting technique consisting of reduction and sulfur-fixation was proposed for study. With single-factor tests, effects of influencing factors, including the proportion of reductants, dosage of sodium carbonate, FeO/SiO2 mole ratio and CaO/SiO2 mole ratio on smelting were investigated. It is found that the following optimal conditions, including addition of 4% Na2 CO3 , 10% of reductant, FeO/SiO2 mole ratio at 1.4, CaO/SiO2 moler ratio at 0.5, resulted in the direct recovery rate of lead up to 91.98%, the content of lead in slag and ferric matte at 0.68% and 4.33% respectively, and a comprehensive sulfur fixation rate at 82.47%. It is shown that such method, being cleaning and efficient with a short technical process, can realize lead recovery and sulfur fixation by one-step smelting.
What problem does this paper attempt to address?