Abstract:Sintering process was divided into three stages:ignition stage,middle stage (from the ending point of ignition to rising point of flue gas temperature) and flue gas temperature rising stage.The emission concentrations of fine particles and the characteristics of each stage were studied by sinter pot test.The results show that the emission concentration of fine particles during ignition stage and middle stage is relatively low,while it achieves a significant increase during the flue gas temperature increasing stage.Besides,the fine particles ds0 =0.7μm from the three sintering stages have different surface morphologys.The fine particles d50 =0.7 μm from the ignition period and middle stage mainly consist of spherical particles without agglomerating phenomenon while the fine particles from flue gas temperature increasing stage consist of random-shaped aggregation,in which the obvious phenomenon of agglomeration is found.The contents of elements like F,S,K,As,and Pb in the fine particles from the flue gas temperature increasing stage are the highest,but the content of Fe is the lowest comparing to the other stages.
What problem does this paper attempt to address?