High extraction of copper from flotation tailings of waste copper-clad laminates by acidophilic iron-oxidizing enrichment

ZHANG Li-juan,LIU Xiao-wen,KANG Xin,CHEN Yan-zhi,ZHOU Wen-gen,SHI Mei-yu,ZHOU Wen-bo,WEN Yong,WANG Wei,ZHOU Hong-bo
DOI: https://doi.org/10.19476/j.ysxb.1004.0609.2015.10.034
2015-01-01
The Chinese Journal of Nonferrous Metals
Abstract:Recycling of the flotation tailings of waste copper-clad laminates was achieved by bioleaching method, the effects of Fe2+ re-addition, leaching time, initial pH and pulp density on the copper extraction were investigated. The results show that an effective copper extraction can be achieved without re-addition of Fe2+within 5 h. The initial pH and pulp density play important roles in copper extraction. Under the optimized condition of initial pH≤2.2 and pulp density 20%?30%, the Cu leaching rate is more than 95%in 5 h without re-addition of Fe2+and acid.