Structure And Thermal Stability Of Zno-Tio2 Core-Shell Nanowires

Sun Menglong,Wang Hongbo,Nie Xianglong,Ma Dayan,Ma Pei,Xu Kewei
2015-01-01
Rare Metal Materials and Engineering
Abstract:ZnO-TiO2 core-shell nanowires were prepared by a thermal reduction method and an atomic layer deposition (ALD) technique. The effects of deposition thickness, deposition temperature and annealing on crystallization and structure of ZnO-TiO2 core-shell nanowires were studied. ZnO-TiO2 core-shell nanowires were characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM) and high-resolution transmission electron microscopy (HRTEM). The results show that TiO2 shell is transformed from amorphous to crystallization with the increasing of the deposition thickness and deposition temperature. After 500 degrees C annealing, the crystallinity of TiO2 shell is improved, but wavy deformation is observed in the fine core-shell nanowires (the diameter of ZnO nanowires < 80 urn). As for amorphous TiO2 shell deposited at 150 degrees C after 500 degrees C annealing, convex grains are formed on the TiO2 shell and the loss of ZnO appears at the ZnO-TiO2 interface.
What problem does this paper attempt to address?