Numerical Simulation and Experiment of Tube-expanding Hydrostatic Extrusion Forming of AZ80 Magnesium Alloy

Xuanbin HUANG,Zhilin WU,Renshu YUAN,Hongming CAI,Mengjun ZHAO
DOI: https://doi.org/10.14158/j.cnki.1001-3814.2017.11.028
2017-01-01
Abstract:The hydrostatic extrusion process of AZ80 magnesium alloy tube was simulated by using Deform-3D software. The effect of extrusion ratio on the forming process of the hydrostatic extrusion was analyzed in detail. The results show that the extrusion load increases with the increase of the extrusion ratio. When the extrusion ratio increases from 1.75 to 2.22, the peak pressure increases from 306 MPa to 375 MPa, and the amplification is 22.5%.The larger the extrusion ratio is, the more severe the shear deformation of the material is, the more favorable the grain refinement of the material is, the greater the pipe flow rate is, and the greater the flow rate difference between the internal and external walls is. Too large internal and external wall flow rate difference is easy to cause pipe cracking. Choosing the extrusion ratio of 1.88, the large diameter AZ80 magnesium alloy tube is successfully fabricated in the 40 MN horizontal hydrostatic extrusion machine. The surface quality of the tube is good, the wall thickness is uniform and there is no obvious defect.
What problem does this paper attempt to address?