Effect of Cu Partitioning Time on Microstructure and Properties of Steel with I&Q&P Treatment

CHEN Liansheng,XU Jinghui,TIAN Yaqiang,ZHENG Xiaoping,SONG Jinying,MI Zhenpeng
DOI: https://doi.org/10.14158/j.cnki.1001-3814.2016.14.067
2016-01-01
Abstract:Through heat treatment process of intercritical annealing & quenching (I&Q) and intercritical annealing & quenching & partitioning (I&Q&P),effects of Cu partitioning behavior and partitioning time on microstructure and mechanical properties of a low carbon steel containing Cu were studied by scanning electron microscopy (SEM),tensile tests,electron microprobe analysis (EPMA) and X-ray diffraction (XRD).The results show that in the process of dual phase heat preservation,C,Cu and Mn partition from ferrite to austenite,and Cu partitioning effect is obvious.The microstructure of the steel treated by I&Q&P process is lath martensite and retained austenite.With the Cu partitioning time increasing,original grain size becomes large,and martensite becomes large,lath becames coarse.The tensile strength decreases gradually,and elongation firstly increases and then descends.The change trend of the residual austenite volume fraction is consistent with that of elongation.When the partitioning time is 40 min,the residual austenite volume fraction and elongation reach the maximum.At this time,the mechanical properties of materials are the best,tensile strength is 1076MPa,and the product of strength and elongation reaches 26254 MPa· %.
What problem does this paper attempt to address?