Preparation and Application of Low Detonation Emulsion Explosive with Honeycomb Structure

Xue-jiao LI,Guang-hong MIAO,Ming YANG,Quan WANG,Hong-hao MA,Zhao-wu SHEN,Wen-yao HUANG,Zhi-xiong BI
DOI: https://doi.org/10.14077/j.issn.1007-7812.2018.02.009
2018-01-01
Abstract:Aiming at the existing problems of explosion welding explosive,glass microspheres are used as sensitizing agent and diluent,by changing the size and content of glass microsphere,the effect of size and content of glass microsphere on detonation properties of emulsion explosive were studied by using electrical measuring methods to measure detonation veloci-ty.Aluminum honeycomb explosive with the detonation velocity of 2530.5m/s was manufactured,and the effect of size and content of glass microsphere on the density and detonation velocity of emulsion explosive was studied.Copper/steel ex-plosion welding was conducted and the bonding quality of the clad plate at the interface was observed by metallographic mi-croscope(OM).The results show that sensitization effect and detonation velocity adjustment effect of glass microsphere with small size(particle diameter:5-100 μm)are good than those of glass microsphere with large size(particle diameter:70-200 μm).When glass microsphere content of emulsion explosive is less than 1% or greater than 40%,the phenome-non of misfire will happen.When glass microsphere content with small size(particle diameter:5-100 μm)is greater than 5% and less than 30%,detonation velocity and density of emulsion explosive respectively decrease from 4915m/s to 1923m/s and from 1.14 g/cm3to 0.70 g/cm3with the increase of glass microsphere content.The critical thickness of alu-minum honeycomb explosive with the detonation velocity of 2530.5m/s is 9mm.The aluminum honeycomb panel can de-crease the critical diameter of emulsion explosive.The interface of copper/steel clad plate shows small wave shape and has good bonding quality.
What problem does this paper attempt to address?