Experimental Study on Iron Separation From a Lead -Zinc Tail in Yunnan Province

Qing-rong YANG,Gui-fang ZHANG,YANPeng
DOI: https://doi.org/10.3969/j.issn.1009-0479.2015.05.005
2015-01-01
Abstract:A lead -zinc mine in Yunnan produces annually 100 000 t of flotation tailings.Flotation tail-ings contains iron 8.72%,sulfur 0.94%,phosphorus 0.14% and other impurities.Direct storage of tailings pile can lead to increase mine cost pressures and waste of resources.The rough concentrate was obtained by using weak magnetic -intensity magnetic separation -flotation desulfurization joint process, where in the flotation process uses a thick and sweep process.H2 SO4 and MHH -1 are mixed as activa-ting agent of pyrite.Experimental studies showed that,qualified iron concentrate could be obtained by a joint process of weak magnetic separation -strong magnetic separation -flotation desulfurization,which the Fe content is 58.02%,the impurities content of sulfur,phosphorus are respectively 0.20% and 0.09%,and comprehensive recovery rate is 70.81%.
What problem does this paper attempt to address?