A surfactant-free preparing method of a CeO2/C nanometer mesh

Yin Shibin,He Shangkai,Wang Peng,Luo Lin,Shen Peikang
2017-01-01
Abstract:A surfactant-free preparing method of a CeO2/C nanometer mesh is disclosed. The method includes (1) weighing a cerium salt, dissolving the cerium salt into water, adding a carbon source into the obtained solution and stirring the solution to obtain a solution mixture of the cerium salt and the carbon source, with the mole ratio of the cerium salt to the carbon source being 1:44.7-1:83.7; (2) transferring the solution mixture obtained in the step (1) into a reactor, performing a hydrothermal reaction, cooling the reactor to obtain a hydrothermal product, and performing middle-period treatment to obtain dried powder; and (3) calcinating the dried powder obtained in the step (2) at 800-1000 DEG C in an inert gas atmosphere for 1-3 h, and cooling the powder to obtain a product. The method is simple in process and high in repeatability. Raw materials adopted are cheap and wide in source, and the final product is a metal oxide-carbon composite material which is nontoxic and environmentally friendly.
What problem does this paper attempt to address?