Improvement in Mechanical and Magnetocaloric Properties of Hot-Pressed La(Fe,Si)13/La70Co30 Composites by Grain Boundary Engineering

X. C. Zhong,D. R. Peng,X. T. Dong,J. H. Huang,H. Zhang,Y. L. Huang,S. M. Wu,H. Y. Yu,W. Q. Qiu,Z. W. Liu,R. V. Ramanujan
DOI: https://doi.org/10.1016/j.mseb.2020.114900
IF: 3.407
2021-01-01
Materials Science and Engineering B
Abstract:Magnetocaloric composites La(Fe,Si)(13)/La70Co30 were fabricated by hot-pressing (HP) followed by annealing. With increasing La70Co30 binder content up to 16 wt%, the maximum compressive strength (sigma(bc))(max) improved dramatically from 63 to 352 MPa. However, the maximum magnetic entropy change (-Delta S-M)(max) decreased from 10.0 to 5.6 Jkg(-1)K(-1) because of the presence of non-magnetic La70Co30. After annealing at 1323 K for 4 h the (sigma(bc))(max) of HP + Annealed composites with up to 12 wt% La70Co30 doubled compared to HP samples. On the other hand, for a La70Co30 content of 16 wt%, the (sigma(bc))(max) of HP + Annealed composites decreased slightly compared to that of HP samples, due to reduced alpha-Fe content and much greater 1:13 phase content in HP + Annealed samples. Remarkably, the (-Delta S-M)(max) of HP + Annealed composites improved from 4.8 to 9.2 Jkg(-1)K(-1) (under 2 T), due to 1:13 phase recombination, after annealing at 1323 K for 4 h.
What problem does this paper attempt to address?