Weld Formation Characteristics in Resistance Spot Welding of Ultra-Thin Steel High welding current and short welding time were found to produce the best combination of strength and weld size

Y. Y. Zhao,Y. S. Zhang,Pei-Chung Wang
IF: 2.2
2017-01-01
Welding Journal
Abstract:Recent trends toward economically fabricating lightweight vehicles while ensuring structural performance makes thin (e.g., <0.5 mm) steels increasingly attractive in the automotive industry. In the present study, the formation of the weld during resistance spot welding (RSW) of a 0.35-mm-thick 600 MPa grade dual-phase steel was investigated. The results indicated the weld initiated early and grew to reach a maximum size of 2.8 mm within a welding time of 40 ms, and then its size remained virtually unchanged, and gradually exhibited a unique "double-layer" feature. Furthermore, the mechanism for the formation of weld layering was modeled from the perspective of temperature evolution. Modeling results indicated the temperature weld zone increased initially but then surprisingly decreased for the remaining welding process, and eventually resulted in a "double-layer" weld. It was found that the strength of the weld increased with the weld size and was improved little with the occurrence of the weld layering. Therefore, the use of high welding current and short welding time is preferable to join ultra-thin steel.
What problem does this paper attempt to address?