NiOxnanoparticles Obtained from Hydrothermally Treated NiC2O4as an Electron Blocking Layer for Organic Photodetectors

Yi Li,Longmei Mao,Longxin Yu,Xifeng Li,Jianhua Zhang
DOI: https://doi.org/10.1088/1361-6528/abb48d
IF: 3.5
2020-01-01
Nanotechnology
Abstract:A room-temperature p-type NiO(x)film synthesized from a NiC(2)O(4)precursor via hydrothermal treatment is employed as an electron blocking layer (EBL) to fabricate organic photodetectors (OPDs). A simple and efficient calcine process at 375 degrees C in air decomposes the NiC(2)O(4)particles into NiOx, removes organic components and crystal water, and releases CO(2)gas. Our experimental results indicate that this gaseous by-product prevents the agglomeration of NiOx, which yields smaller nanoparticles (5-10 nm). The formation of an EBL at room temperature improves device performance. After optimization, the performance parameters obtained, including dark current density, responsivity, specific detectivity and response, are 1.13 x 10(-7)A cm(-2), 0.74 A W-1, 3.86 x 10(12)Jones, and 0.5/8 ms, respectively. Additionally, the dark current is reduced by more than an order of magnitude after the insertion of the NiO(x)layer. The proposed simple and easy method for producing an EBL could be beneficial for the commercial low-temperature and large-area preparation of OPDs.
What problem does this paper attempt to address?