Pyridinium group containing moderate polarity skeleton adsorption resin and preparation method thereof

Cai Jianguo,Lv Lu,Zhang Weiming,Pan Bingcai,Zhao Xin,Lin Yuan,Su Shuangxi
2013-01-01
Abstract:The invention discloses a pyridinium group-containing moderate-polarity skeleton adsorption resin and a preparation method thereof, and belongs to the technical field of polymer adsorption resin. The resin has the grain size of 0.3-0.85mm, the water content of 55 to 70 percent, the weak basic exchange capacity of 1.0-4.0mmol/g, the specific surface area of 200-750m /g and the average pore size of 3-12nm. The preparation method comprises the following steps: 1, dissolving a dispersing agent and NaCl in water to obtain an aqueous phase; 2 making vinylpyridine, a cross-linking agent, a pore-forming agent, a regulator and an initiator form an organic phase; and 3, sequentially adding the aqueous phase and the organic phase into a reactor, introducing nitrogen to remove oxygen from the reactor, stirring until the organic phase is dispersed to proper grain size in the aqueous phase and temperature rise reaction is carried out, cooling to room temperature, steaming out the pore-forming agent, washing and drying. The resin has a good effect of removing organics with moderate polarity and polarity, and can be used for treating related wastewater; and synthesis steps for the resin are simple, and the monomer conversion rate is high.
What problem does this paper attempt to address?