Effect of the debinding method on the properties of injection molding ceramics

Yin Wu,Wenjie Si,Hezhuo Miao
DOI: https://doi.org/10.3321/j.issn:1002-185X.2005.09.033
2005-01-01
Rare Metal Materials and Engineering
Abstract:This paper, supercritical CO2 debinding, solvent immersion and thermal treatment were used to remove binder from ZrO2 ceramic injection molded (CIM) green parts. The properties of the sintered sample debinded by the three methods were compared. Results show that the debinding methods have considerable influence on the properties of sintered samples because of the different mechanisms of the methods. By supercritical CO2 debinding, the defects occurred in thermal debinding can be avoided and the mechanical properties can be improved. The values of bending strength and Weibull modulus of the sintered samples by supercritical debinding (sigma-1074 MPa, m=18.93)are higher than those obtained by solvent debinding (sigma=1038.4 MPa, m=13.28) or by thermal treatment (sigma=983.5 MPa, m=7.59). Moreover, with supercritical and solvent debinding, the debinding time can be reduced greatly to about one twentieth of the time required by thermal debinding.
What problem does this paper attempt to address?