Lead leaching characteristics of CRT leaded glass and its slag after lead extraction by smelting

Xie,Fang-Fang,Ou,Zhi-Yuan,Li,Jin-Hui,Liu,Li-Li
2014-01-01
Abstract:Evaluating the environmental impact of different cathode ray tube (CRT) leaded glass parts and its slag after lead extraction by smelting was helpful for the recycling and disposal of CRT glass. This study investigated the Pb leaching characteristics of different leaded CRT glass parts and its slag after lead extraction by HJ/T300-2007. The results showed lead leaching concentrations of funnel, panel, and frit glass all exceeded the threshold of leaching concentration for hazardous waste, and lead in frit glass was very easy to leach, contributing most to CRT toxicity;lead in slag was also very easy to leach, and leaded slag could be regarded as general solid waste only if its lead concentration was below 1.5%. Except for the Pb content in the material, Pb structure contributed a lot to the difference of Pb leaching.