Investigations into the influence of nickel loading on MoO 3 -modified catalysts for the gas-phase hydrodeoxygenation of anisole

Simon Haida,Sebastian Löbner,Henrik Lund,Stephan Bartling,Carsten Robert Kreyenschulte,Hanan Atia,Ali M. Abdel-Mageed,Christoph Kubis,Angelika Brückner
DOI: https://doi.org/10.1039/d3cy01488f
IF: 6.177
2024-03-06
Catalysis Science & Technology
Abstract:Molybdenum oxide-based catalysts are promising catalysts for the gas-phase hydrodeoxygenation (HDO) of lignocellulosic pyrolysis oils with high selectivities to arenes. The gas-phase HDO is conducted at temperatures between 300 °C and 400 °C at ambient pressure, resulting in a low hydrogen consumption and high energy efficiency. The loading by nickel forming a binary structure consisting of MoO 3 and nickelmolybdate (NiMoO 4 ) during calcination, resulting in a significant increase of the catalytic activity connected with a drastic shortening of the induction period observed for the unpromoted catalyst system. The promotional effect of nickel seems to be related to its enhanced reduction behaviour and hydrogen dissociation leading eventually to an improved formation of a molybdenum oxycarbohydride phase (MoO x C y H z ). The MoO x C y H z phase plays an important role in stabilizing active Mo 5+ sites and prevents over-reduction to inactive MoO 2 . The activity and benzene selectivity is maximal when the pure NiMoO 4 is used as catalyst. However, the selectivity towards undesired methane increases significantly indicating a decomposition of arenes. This effect is considerably reduced for catalysts with lower nickel contents (3-5 %) which still exhibit a highly improved activitiy compared to MoO 3 . In-situ XRD studies revealed that the population of the MoO x C y H z phase is strongly affected by the nickel content, the structure of the hydrocarbon substrate and the hydrogen content during pre-reduction and catalysis.
chemistry, physical
What problem does this paper attempt to address?