Abstract:B-containing high temperature titanium alloys were in situ fabricated successfully by casting route. The influences of heat treatment processes on the evolution of microstructures, textures, strengths, elongations and fracture characteristics at room temperature (RT) and high temperature (650 degrees C) were analyzed. Microstructure investigation revealed that TiB whiskers stimulated the dynamic recrystallization behavior. The volume fractions of primary alpha phase (V-P alpha) decreased with the increasing solution temperature, while the volume fractions of transformed beta phase (V-T beta) and widths of secondary alpha lamellas in transformed beta phase (W-S alpha) increased. The inverse pole figures (IPFs) observations illustrated nea-requiaxed alpha grains transformed to ideal equiaxed morphology after 960 degrees C solution. By the analyzation of pole figues (PFs), after alpha+beta heat treatments, the overall texture intensity increased with the increasing solution temperature, and after beta heat treatments, textures with comparatively high intensities were concentrated around various directions. The equiaxed alpha grains and lamellar alpha phase had similar main texture components. But the maximum texture intensity of lamellar alpha phase was obviously higher than that of equiaxed alpha grains. Moreover, the textures of equiaxed alpha gains and lamellar alpha phase exhibited higher similarity after 980 degrees C solution comparing with after 960 degrees C solution. Alloy after 980 degrees C solution exhibited an excellent combination of RT and 650 degrees C mechanical properties which was ascribed to the microstructure tailoring and the load-sharing effect of TiB whiskers. Fracture of alloys was due to the debonding of TiB whiskers, and the growth and coalescence of micro-voids in matrix and around the cracks of fractured TiB whiskers. (C) 2019 Elsevier B.V. All rights reserved.
What problem does this paper attempt to address?