Temperature Dependent Fracture Toughness of KNN-Based Lead-Free Piezoelectric Ceramics

Yingwei Li,Yixuan Liu,Paul-Erich Oechsner,Daniel Isaia,Yichi Zhang,Ke Wang,Kyle G. Webber,Jing-Feng Li,Juergen Roedel
DOI: https://doi.org/10.1016/j.actamat.2019.05.060
IF: 9.4
2019-01-01
Acta Materialia
Abstract:The fracture toughness of lead-free KNN-based piezoelectric ceramics with the composition of 0.92KNN-0.02Bi0.5Li0.5TiO3-0.06BaZrO3 was investigated by near-tip crack opening displacement (COD), surface crack in flexure (SCF), as well as single edge V-notch beam (SEVNB) techniques. Results reveal that the intrinsic fracture toughness (KI0), evaluated by the COD technique, is the lowest with a value of 0.70 MPa∙m0.5. The long (through-thickness) crack fracture toughness (KIvnb), obtained by the SEVNB technique, is the highest, with a value of 0.95 MPa∙m0.5. Intermediate short surface crack fracture toughness (KIsc) of 0.86 MPa∙m0.5 was determined by the SCF technique. These results were rationalized by the toughening behavior of the material combined with the crack geometry-dependent stress intensity evolution during crack propagation. With increasing temperature, KIvnb and KIsc decrease. At 350 °C, they are nearly identical, suggesting an absence of toughening. Nonlinear stress-strain analysis of the material was also employed during compression and four-point bending in order to quantify crack tip shielding by domain switching and in order to quantify the actual stress at the point of instable crack propagation.
What problem does this paper attempt to address?