Evaluation of TZM/ZrCp-W Joint Brazed with Ti-35Ni Filler: Microstructure and Mechanical Properties

X. G. Song,G. H. Han,S. P. Hu,H. Y. Zhao,Y. Li,M. R. Wang,B. Shi
DOI: https://doi.org/10.1016/j.msea.2018.11.017
IF: 6.044
2018-01-01
Materials Science and Engineering A
Abstract:To broaden the application of the Titanium-Zirconium-Molybdenum alloy (TZM) and the ZrC ceramic particle reinforced tungsten composite (ZrCp-W) in the elevated temperature fields, the two materials were brazed with Ti-35Ni filler. The interfacial microstructure of the TZM/Ti-35Ni/ZrCp-W joint was divided into three zones: a reaction zone I containing Mo, Ti-Mo solid solution and Ti2Ni; a brazing seam II composed of TiNi phase and Ti2Ni phase; a diffusion layer III consisting of tungsten and (Ti, Zr)C particles fixed by Ti-Ni alloy. With the increase of temperature, in zone I, the micromorphology turned rougher, and the Ti-Mo and Ti-Ni stripes turned more and wider; the brazing seam gradually narrowed and eventually disappeared. A new phase TiC was generated in zone III, and the content of TiC in zone III increased, whereas the content of Ti2Ni decreased. When brazed at 1260 degrees C for 10 min, the fracture originated and extended at the TZM side, and the maximum mean shear strengths of 123.8 MPa at room temperature and 110.2 MPa at 800 degrees C were gained, respectively, the fracture surface were characterized by inter-granular fracture. Meanwhile, the continuous Ti2Ni phase and the wider Ti-Ni stripes will reduce the joints properties.
What problem does this paper attempt to address?