Effects of solid-state polycondensation temperature and time on PET crystallinity

Li Jinxia,Shen Xijun,Feng Lianfang,Zhang Jun,Wang Jiajun
DOI: https://doi.org/10.3969/j.issn.1001-0041.2006.03.007
2006-01-01
Abstract:The changes of intrinsic viscosity and crystallinity with reaction conditions were studied for polyethylene terephthalate ( PET) chips during solid-state polycondensation. The thermal behavior of PET chips was also analyzed. The results showed that the intrinsic viscosity of PET chips was increased with the reaction temperature and time and was optimized in the range of 215-225℃. The crystallization occurred while the reaction proceeding and slowed down to equilibrium after a fixed period of time. The DSC curves showed that a characteristic melt peak at about 253℃ and a solid-state polycondensation peak were observed for PET after solid-state polycondensation. The solid-state polycondensation peak shifted towards the characteristic melt peak while increasing reaction temperature and time, then became a single peak at a specific reaction temperature and time, and finally moved to high temperature range from low temperature range, separating from the characteristic melt peak.
What problem does this paper attempt to address?