Synthesis of LiFePO4 by solvothermal method as cathode materials for lithium iron batteries

Fei CHENG,Qiang SUN,An-hui LU,Wen-cui LI
DOI: https://doi.org/10.3969/j.issn.1002-087X.2013.05.011
2013-01-01
Abstract:LiFePO4 was prepared by a solvothermal method in a water-polyethylene glycol (PEG400) binary solvent using ascorbic acid (VC) as reducing agent. The structure, morphology, and properties of the samples were characterized by XRD, SEM and TG. The results show that the addition of VC can prevent the oxidation of divalent iron, more importantly, the crystal shape and discharge capacity varied with VC content. With the coaction of VC and PEG400, the pure LiFePO4 can deliver a discharge specific capacity of 143.2 mAh/g at 0.1 C. Over 20 cycles, the electrode can maintain 74.4% of its initial capacity. After heat treatment, the residual PEG400 on the surface of LiFePO4 was converted into carbon, which made the charge-discharge capacity and the cycle performance further improved and avoided the structural defects and non-uniform of carbon coating layer caused by the process of milling. Over 30 cycles, the electrode showed 97% capacity retention compared to an initial capacity and the coulombic efficiency stayed at about 100%.
What problem does this paper attempt to address?