Research on Casting Process for Embedded Internal Flow Passage Mould

单忠德,叶永盛,王宝雨,姜超,闫沁太
2014-01-01
Abstract:In the casting process of embedded internal flow passage mould, the collapse and deformation were prone at high temperature due to thin wall(2~6 mm) and narrow tube(10~20 mm), which cause the blockage in the internal flow passage and cannot guarantee the liquidity of internal flow passage. Aiming at this problem, adopting numerical simulation analysis mould, and taking four kinds of medium which include nothing filling, zircon sands, iron powder and Ar to fill seamless steel tube(准18 mm×4 mm), the temperature-time curves of different position in casting process were obtained, and the reliability of numerical simulation was verified by experimental. The results show that the hollow tubes reach the peak of 1 369 ℃ in 2 min and there are the passage collapse and deformation in the casting process. When filling the zircon sands, there are not the passage collapse and deformation, so as to ensure the liquidity of internal flow passage.
What problem does this paper attempt to address?