Factors affecting photocatalytic activity of visible light-responsive titanium dioxide doped with chromium ions

Naoto Nishiyama,Keisuke Kozasa,Toshihiro Okajima,Mamoru Fujitsuka,Tetsuro Majima,Suzuko Yamazaki
DOI: https://doi.org/10.1039/c8cy01411f
IF: 6.177
2018-01-01
Catalysis Science & Technology
Abstract:Titanium dioxide doped with Cr ions (Cr-TiO2) was synthesized by a sol-gel method, with only water as the solvent, and dialysis. For Cr-TiO2 sintered at 200 degrees C, ca. 90% of 4-chlorophenol (4-CP) was degraded at Cr doping amounts of 0.68-1.3 atom% under visible light irradiation. At doping amounts above 1.7 atom%, the 4-CP degradation ratio increased for Cr-TiO2 sintered at 300-500 degrees C. X-ray photoelectron spectroscopy and X-ray absorption near edge structure measurements showed that only Cr(iii) was present on the surfaces of Cr-TiO2 samples sintered at 200 or 400 degrees C and some of the Cr(iii) in the bulk was oxidized to Cr(vi) by sintering at 400 degrees C. The 4-CP degradation was enhanced with increasing Cr(vi)/Cr(iii) ratio in the bulk, suggesting the spatial separation of Cr(iii) on the surface under visible light irradiation: electrons are excited from Cr(iii) to the conduction band of TiO2 and then trapped at the doped Cr(vi) whereas the photogenerated Cr(iv) oxidizes 4-CP. Time-resolved diffuse reflectance spectroscopy was used to evaluate the lifetimes of the photogenerated electrons. The highest photocatalytic activity was obtained with ca. 0.8 atom% Cr-TiO2 sintered at 200 degrees C. This high activity is ascribed to the presence of oxygen vacancies, which act as electron-trapping sites.
What problem does this paper attempt to address?