He Behavior in Ni and Ni-based Equiatomic Solid Solution Alloy

Zhanfeng Yan,Shaoshuai Liu,Songqin Xia,Yong Zhang,Yugang Wang,Tengfei Yang
DOI: https://doi.org/10.1016/j.jnucmat.2018.04.009
IF: 3.555
2018-01-01
Journal of Nuclear Materials
Abstract:In the current work, pure nickel (99.99 wt.%) and Ni-containing single phase equiatomic solid solution alloy Fe-Co-Cr-Ni were irradiated with 190 keV He ions at room temperature with different fluences and He behavior in both materials are compared. At 1 x 10(17) cm(-2), TEM observation reveals that only isolated and small He bubbles (1-2 nm) are formed in Fe-Co-Cr-Ni alloy while many small suspected "string"-like He bubbles are observed in nickel at the concentration peak region (5.5 at.%). When the fluence is increased to 5 x 10(17) cm(-2), average bubble size in nickel increases to similar to 8 nm which is almost equal to that in Fe-Co-Cr-Ni, but a higher bubble density is observed in nickel. At the highest dose of 1 x 10(18) cm(-2), numerous surface blisters and exfoliations occur in nickel which are consistent with TEM observation, while the Fe-Co-Cr-Ni alloy only shows a slight surface blister. Bubble coarsening upon annealing at 500 degrees C (2 h) is observed at 5 x 10(17) cm(-2) in both alloys, but a significant larger bubble growth is observed in nickel, suggesting a relatively better resistance to He bubble growth for Fe-Co-Cr-Ni alloy. (C) 2018 Elsevier B.V. All rights reserved.
What problem does this paper attempt to address?