Synthesis of Phenol Formaldehyde (PF) Resin for Fast Manufacturing Laminated Veneer Lumber (LVL)

Shu Hong,Zhongji Gu,Ling Chen,Ping Zhu,Hailan Lian
DOI: https://doi.org/10.1515/hf-2017-0184
2018-01-01
Holzforschung
Abstract:Abstract Phenol formaldehyde (PF) resin is a well-tried adhesive for manufacturing laminated veneer lumber (LVL). PF has a high bonding strength, good cold pressing property and contributes a lot to the high production efficiency of LVL. In the present paper, PFs were synthesized at three different alkaline condition levels with a molar formaldehyde to phenol (F/P) ratio of 2.25. The bonding strength of PFs was not influenced by the alkalinity. Compared with PFs synthesized under alkalinity of 1 and 4%, PF with 8% alkalinity formed a resin with a high mole mass (MM), uniform mole mass distribution (MMD) and a high cross-linking density. With PF8%, the cold pressing property could be shortened from 30 to 12 min in the winter time. Cured PF8% had a higher cross-linking density than PF1% and PF4%. PF8% has a high potential for industrial production of LVL.
What problem does this paper attempt to address?