Preparation of High Catalytic Activity Biochar from Biomass Waste for Tar Conversion

Peng Lu,Qunxing Huang,Yong Chi,Jianhua Yan
DOI: https://doi.org/10.1016/j.jaap.2017.09.003
IF: 6
2017-01-01
Journal of Analytical and Applied Pyrolysis
Abstract:High catalytic activity biochar from biomass waste by co-processing of H2O/CO2 activation and nickel loading for the conversion of tar model compound (toluene) were prepared. Raw char was produced by pyrolyzing pine wood sawdust at 800 degrees C for 1 h, then activated by CO2 or H2O (15 vol.% in N-2) at 800-900 degrees C for 20-80 min. The nickel loading amount was 2 mmol/g-char (11.74 wt.%). The catalytic cracking of toluene was carried out in a lab-scale fixed bed reactor at 800 degrees C with a residence time of 0.13 s. The results showed that activation significantly improved the average toluene conversion from 40.1% by raw char to 93.2% by activated char (H80). High porosity and hierarchical pore structure, more defects in graphene-like carbon structure and oxygen containing groups on the surface (C-O) contributed to the higher catalytic activity of activated chars. The nickel loading increased the toluene conversion of raw char (Ni-char) and activated char (Ni-C900) from 40.1 to 80.8% and from 77.7 to 94.9%, respectively, due to the additional supply of active sites. The toluene conversion ratio of Ni-C900 was larger than that of Ni-char due to a more uniform dispersion of nickel on the activated char support. Thus, the raw biochar should be initially activated before used as catalyst or catalyst support to obtain a higher and more stable catalytic activity for tar conversion.
What problem does this paper attempt to address?