Microstructural Evolution of TP347H After Post Weld Heat Treatment and Aging

Chao Fang,Kejian Li,Houyu Ma,Yinsheng He,Keun-Bong Yoo,Jinesung Jung,Keesam Shin
DOI: https://doi.org/10.1166/sam.2016.2881
2016-01-01
Science of Advanced Materials
Abstract:Nb-stabilized TP347H stainless steel is widely used as reheater and superheater components in a power plant setting. Because of the extreme environment of high temperature and high pressure due to steam in power generation, material degradation and failure can occur, especially in the heat-affected zone (HAZ). This presents an urgent problem that requires immediate attention to ensure the safe and effective long-term operation of power plants. In this study, as-fabricated specimens of TP347H were welded using a two-pass welding process with subsequent post-weld heat treatment (PWHT). Next, both the as-welded and PWHT specimens were subjected to an aging test at 600 degrees C for 100 hrs, 400 hrs, or 1000 hrs. The experimental results suggest PWHT effectively retards the precipitation of M23C6 along the grain boundary, preventing the weakening of grain boundaries due to Cr depletion by the formation of M23C6. Therefore, PWHT is an effective measure for the prevention of premature failure of TP347H weld joints.
What problem does this paper attempt to address?