Fouling Formed on SS316L Tube Surface from Thermal Oxidative Degradation of Exo-Tetrahydrodicyclopentadiene

Maogang He,Qian Zhang,Xiangyang Liu
DOI: https://doi.org/10.1016/j.applthermaleng.2017.02.118
IF: 6.4
2017-01-01
Applied Thermal Engineering
Abstract:Exo-tetrahydrodicyclopentadien called JP-10 is an endothermic hydrocarbon fuel with high-energy density being used in aircrafts. We have investigated the fouling of JP-10 on the inner surface of SS316L tube at wall temperature from 260 degrees C to 350 degrees C and at 3.84 MPa with a flow rate of 0.5 ml/min for 24 h. The fouling of JP-10 was influenced by wall temperature, fuel temperature and the metal surface. The average values of coke deposits were measured to be between 7.52 mu g/cm(2) and 10.67 mu g/cm(2) by carbon burn-off method, and the maximum values of local coke deposits and average values of coke deposits increase with the wall temperature. At 350 degrees C and 300 degrees C, the locations of peak deposition shifted upstream as the wall temperature increased. The nature and morphology of deposits were characterized by field emission scanning electron microscopy (FESEM) and temperature programmed oxidation (TPO) profiles, and the deposits of JP-10 were mainly in the form of amorphous carbon. Structurally more ordered deposits were also found, and it should be caused by the catalysis of iron and nickel in metal surface. (C) 2017 Elsevier Ltd. All rights reserved.
What problem does this paper attempt to address?