Oxidation behavior of the directed energy deposited 316 L stainless steel in supercritical carbon dioxide environment: effect of post-manufacturing heat treatment

Junjie Chen,Hyeon Bae Lee,Chaewon Jeong,Qian Xiao,Kyungnam Jang,Taejeong An,Changheui Jang
DOI: https://doi.org/10.1016/j.addma.2024.103998
IF: 11
2024-01-26
Additive Manufacturing
Abstract:The oxidation behaviors of directed energy deposit (DED) 316 L SS with various post-DED heat treatments (HTs) as well as commercial 316 L SS were investigated in a 650 °C/20 MPa sCO 2 environment. In addition to the detailed microstructure analyses, ultraviolet photoelectron spectroscopy (UPS) analysis was performed to measure the valence electron configuration, and the results were considered in understanding the observed oxidation behavior. Compared to commercial 316 L SS, the unique large columnar grains and decrease in valence electron density of DED 316 L SS benefit the oxidation resistance by retarding cation and anion migrations, even though they have similar oxide layer consisting of a Fe-rich outer oxide layer and a Cr- and Fe-rich internal oxidation zone. After stress-relieving HT at 850 °C, the oxidation resistance is further enhanced owing to the HT-induced dislocation density decrease, resulting in a thinner sandwich-like oxide layer with chromia-type outer and inner sublayers and a silicon oxide middle sublayer. Additional improvement in the oxidation resistance is observed after homogenization HT at 1150 °C, with a thinner oxide layer and less inward intergranular oxidation, which could be attributed to an additional decrease in valence electron density.
engineering, manufacturing,materials science, multidisciplinary
What problem does this paper attempt to address?