Production of high purity rare earth mixture from iron-rich spent fluid catalytic cracking (FCC) catalyst using acid leaching and two-step solvent extraction process
Le-Phuc Nguyen,Yen Thi Hai Pham,Phuong Thuy Ngo,Tri Van Tran,Loc Vinh Tran,Nam Thi Hoai Le,Luong Huu Nguyen,Tung Thanh Dang,Duc Anh Nguyen,Marco Wenzel,David Hartmann,Karsten Gloe,Jan J. Weigand,Klaus Kretschmer
DOI: https://doi.org/10.1007/s11814-018-0022-z
IF: 2.7
2018-03-23
Korean Journal of Chemical Engineering
Abstract:Acid leaching and a two-step solvent extraction procedure were developed to produce high purity mixture of La and Ce from iron-rich spent FCC catalyst discharged from Dzung Quat refinery (Vietnam). Acid leaching of the spent catalyst with 2M HNO3 and a solid-to-liquid ratio of 1/3 at 80 °C in 1 h dissolved almost 90% of La while 12% of Al and 25% of Fe were transferred to the leachate. The extraction of RE metals and main impurities such as Al and Fe by a mixture of di-2-ethylhexyl phosphoric acid (D2EHPA) and tributyl phosphate (TBP) was investigated. Experiments showed that it was necessary to remove Fe before extracting RE and the optimum extraction conditions for a high recovery of RE while 0% of Al extraction were pH-1, contact time=10min, and D2EHPA/TBP volume ratio= 4: 1. At these conditions, the extraction yields of La(III) and Ce(III) were 72% and 89%, respectively. A two-step solvent extraction was developed to achieve a high purity of RE mixture, which included (1) the removal of impurity Fe by 25% (v/v) diisooctyl phosphinic acid (DiOPA) in n-octane for 140 min, (2) the extraction of rare earths by a mixture of di-2-ethylhexyl phosphoric acid (D2EHPA) and tributyl phosphate (TBP) in n-octane for 10 min without the need for adjusting the pH of the leaching solution.
engineering, chemical,chemistry, multidisciplinary