Mechanical Properties of Laser Welds of Nickel-Chromium Alloy in Dentistry by Pulsed Nd:YAG Laser Apparatus

刘红,朱松,李蕾,欧阳喈,刘俐,方鸣岗
DOI: https://doi.org/10.3969/j.issn.1003-7632.2002.05.016
2002-01-01
Abstract:Objective The mechanical properties of laser-welded nickel-chromium alloy under different laser welding conditions were evaluated to find the optimal parameters.Methods Different laser irradiation power was used to weld dental nickel-chromium alloy by Nd:YAG apparatus. Mechanical properties, metallographic evaluation and scanning electron microscopy (SEM) analysis were used to evaluate joined samples.The mechanical properties,including tensile strength,percentage elongation and Vickers microhardness, were compared with parent samples.Results Mechanical properties was improved simply by increasing the irradiation power. Tensile strength of joined samples irradiated by laser at 10.5 Joules were similar to that of the original metal.No statistically significant difference was found between joints fused at 10.5 Joules and the parent mental.Compared with original metal,the elongation values of joined samples decreased significantly.The microhardness values increased in the welded joint region. SEM observation on fracture surface revealed that the most penetration depth was 0.9 mm to 1.0 mm.No porosities and cracks and other defects were found.Conclusion Laser welding has stronger welded joints and smaller heat-affected zone and greater penetration depth. Nd:YAG laser welding of nickel-chromium alloy could get a good result through selecting appropriate parameters.
What problem does this paper attempt to address?