Abstract:In-situ composite of Zn-27Al-6.3Mg-3.7Si alloy was fabricated by centrifugal casting using the heated permanent mold. This kind of composite is consisted of three layers, inner layer segregates lots of blocky primary Mg_2Si and a little blocky primary Si, middle layer contains no primary Mg_2Si and primary Si, outer layer contains a little. Zn-27Al-6.3Mg-3.7Si alloy solidifies according to following steps: firstly, the precipitation of primary Si and primary Mg_2Si, secondly, the precipitation of Zn-phase enriched by Al, thirdly, the precipitation of Mg-Zn compound, and lastly, the occurrence of ternary or quaternary eutectic reaction. The position, quantity and distribution of primary Mg_2Si and primary Si are determined by solidification velocity under the effect of centrifugal force and their floating velocity inward. The inner and outer layer contained primary Mg_2Si and primary Si exhibit much higher hardness and wear resistance than the middle layer.
What problem does this paper attempt to address?