Grain Refinement of Wrought Magnesium Alloy and Microstructures and Properties in Annealing States

宋孚群,张青来,徐永超,张坤,张士宏,王忠堂
DOI: https://doi.org/10.3969/j.issn.1674-6457.2004.03.015
2004-01-01
Abstract:Plasticity property of magnesium alloy was improved with grain refinement in the process of deformation. Extrusion thinner strip was obtained with fine grains for size of 2.5~12.5μm in high extrusion ratio 100:1; high extrusion ratio and rolling ensured thinner strip of magnesium alloy with average size of grains less then 5 μm. The best microstructure and mechanical properties of magnesium alloy were gained by optimal recrystallization annealing. High hot drawing property of fine grain strip was presented after hold time 20min at 523K, and then fine grain strip successfully attained qualified cup-rawing, however poor hot drawing appeared for size of grains above 25μm.