Effects of Phytic Acid on Protective Performance of Film Formed on Pure Magnesium by Ultrasonic Micro-arc Oxidation

WEI Fang-hong,LI Mu-qin,GUO Xiao-juan,LI Yong-jiang
DOI: https://doi.org/10.11933/j.issn.1007-9289.2015.02.008
2015-01-01
China surface engineering
Abstract:To decrease the perfoliate pore of the oxide film througth the ultrasonic micro-arc oxidation,phytic acid were adopted as conversion treatment.Its effect on protective performance of the film formed on pure magnesium by ultrasonic micro-arc oxidation were researched.The surface morphology,functional group and protective performance of mic-arc oxidation film before and after treated by phytic acid were studied by SEM,EDAX,fourier infrared spectrometer(FTIR)and electrochemical corrosion workstations,respectively.The results show that with the increasing of the phytic acid concentration,the pore amount of ultrasonic micro-arc oxidation film decreases,uniform density and coverage increases,and the film surface is rich in phosphate and hydroxyl.The samples show the best protective performance with most positive corrosion potential and lowest corrosion current and C and P element content on the film are the highest,while Mg element content is the lowest when the concentration of phytic acid is 7.5g/L.Besides the formation mechanism of phytic acid conversion coating was also discussed.
What problem does this paper attempt to address?