Tribological Behavior of Ti3SiC2 and Ti3SiC2/Pb Composites Sliding Against Ni-based Alloys at Elevated Temperatures

Rui Zhang,Keqin Feng,Junhu Meng,Fuyan Liu,Shufang Ren,Wanxiu Hai,Aijun Zhang
DOI: https://doi.org/10.1016/j.ceramint.2016.01.099
IF: 5.532
2016-01-01
Ceramics International
Abstract:The Ti3SiC2 and Ti3SiC2/Pb composites were tested under dry sliding conditions against Ni-based alloys (Inconel 718) at elevated temperatures up to 800°C using a pin-on-disk tribometer. Detailed tribo-chemical changes of Pb on sliding surface were discussed. It was found that the tribological behavior were insensitive to the temperature from 25°C (RT) to 600°C (friction coefficient ≈0.61–0.72, wear rate ≈10−3mm3 N m−1). An amount of Pb in the composites played a key role in lubricating with the temperature below 800°C. The friction coefficient (≈0.22) and wear rate (≈10−7mm3 N m−1) at elevated temperatures were both decreased by the added PbO. The wear mechanisms of Ti3SiC2/Pb-Inconel 718 tribo-pair at elevated temperatures were believed to be the combined effect of abrasive wear and tribo-oxidation wear. During the sliding, two oxidization reactions proceed, 2Pb+O2=2PbO (below 600°C) and 6PbO+O2=2Pb3O4 (800°C). The friction coefficient and wear rate of the composites were reduced due to the self-lubricating effect of the tribo-oxidation products.
What problem does this paper attempt to address?