Low-Viscosity Route to High-Molecular-Weight Water-Soluble Polymers: Exploiting the Salt Sensitivity of Poly( N -acryloylmorpholine)
Rory J. McBride,Elisa Geneste,Andi Xie,Anthony J. Ryan,John F. Miller,Adam Blanazs,Christine Rösch,Steven P. Armes,Christine Rösch
DOI: https://doi.org/10.1021/acs.macromol.3c02616
IF: 5.5
2024-02-23
Macromolecules
Abstract:<p></p><p>We report a new one-potlow-viscosity synthetic route to high molecularweight non-ionic water-soluble polymers based on polymerization-inducedself-assembly (PISA). The RAFT aqueous dispersion polymerization of N-acryloylmorpholine (NAM) is conducted at 30 °C usinga suitable redox initiator and a poly(2-hydroxyethyl acrylamide) (PHEAC)precursor in the presence of 0.60 M ammonium sulfate. This relativelylow level of added electrolyte is sufficient to salt out the PNAMblock, while steric stabilization is conferred by the relatively shortsalt-tolerant PHEAC block. A mean degree of polymerization (DP) ofup to 6000 was targeted for the PNAM block, and high NAM conversions(>96%) were obtained in all cases. On dilution with deionized water,the as-synthesized sterically stabilized particles undergo dissociationto afford molecularly dissolved chains, as judged by dynamic lightscattering and <sup>1</sup>H NMR spectroscopy studies. DMF GPC analysisconfirmed a high chain extension efficiency for the PHEAC precursor,but relatively broad molecular weight distributions were observedfor the PHEAC–PNAM diblock copolymer chains (M<sub>w</sub>/M<sub>n</sub> > 1.9). This has beenobserved for many other PISA formulations when targeting high core-formingblock DPs and is tentatively attributed to chain transfer to polymer,which is well known for polyacrylamide-based polymers. In fact, relativelyhigh dispersities are actually desirable if such copolymers are tobe used as viscosity modifiers because solution viscosity correlatesclosely with M<sub>w</sub>. Static light scatteringstudies were also conducted, with a Zimm plot indicating an absolute M<sub>w</sub> of approximately 2.5 × 10<sup>6</sup> g mol<sup>–1</sup> when targeting a PNAM DP of 6000. Finally,it is emphasized that targeting such high DPs leads to a sulfur contentfor this latter formulation of just 23 ppm, which minimizes the cost,color, and malodor associated with the organosulfur RAFT agent.</p>
polymer science