Synthesis temperature dependence of the structural and electrochemical properties of Mg 2 Si anodic materials prepared via a hydrogen-driven chemical reaction

Yanping He,Yongfeng Liu,Ruijun Ma,Mingxia Gao,Hongge Pan
DOI: https://doi.org/10.1007/s11581-015-1457-4
IF: 2.961
2015-01-01
Ionics
Abstract:To obtain the optimal hydrogen-driven chemical reaction process for the preparation of Mg 2 Si as an anodic material of Li-ion batteries, the effects of the dehydrogenation temperatures on the structure and electrochemical properties are systematically investigated. The results indicate that Mg 2 Si prepared by isothermal dehydrogenation at 310 and 330 °C exhibit better cycling stability than the samples prepared at 290 and 350 °C due to the joint effects of the product purity and the particle size, especially for the 330 °C-prepared sample. In particular, the initial discharge capacity of the Mg 2 Si prepared at 330 °C is 1010 mAh/g with a coulombic efficiency of 92 %. After 50 cycles, the discharge capacity is approximately 416 mAh/g and the corresponding capacity retention is calculated to be approximately 41 %.
What problem does this paper attempt to address?