Flow behaviour of a two phase titanium alloy with lamellar microstructure during subtransus deformation

yan liu,bing de wang,c l bao
DOI: https://doi.org/10.1179/1432891714Z.0000000001275
2015-01-01
Materials Research Innovations
Abstract:Subtransus deformation behaviour of Ti-6.5Al-1.5Zr-3.5Mo-0.3Si alloy with a lamellar structure was studied using isothermal hot compression tests under the deformation temperature range 890-995 degrees C and strain rate range 0.01-10 s(-1). All of the flow curves exhibited a peak stress at very low strains (around 0.05) followed by considerable flow softening. The TEM results of compressed specimen verified dislocation pile-ups at the alpha/beta interfaces which act as grain boundary strengthening, and calculated flow softening degree by the modified model for grain boundary/interface strengthening developed by Semiatin agreed well with the experimental results. Thus the flow softening can be related to reduction with increasing strain of Hall-Petch strengthening by the alpha/beta interfaces. Then a new constitutive equation was developed for subtransus deformation of Ti-6.5Al-1.5Zr-3.5Mo-0.3Si alloy with lamellar structure by combining the Estrin and Mecking model for strain hardening and an empirical model for flow softening.
What problem does this paper attempt to address?