Effect of high bismuth deficiency on structure and oxide ion conductivity of a Bi0.55MoO4 single crystal

yang zhang,hengjiang cong,nianjing ji,jian liu,xiulan duan,jing li,wenwu cao,jiyang wang,huaidong jiang
DOI: https://doi.org/10.1039/c5ce01765c
IF: 3.756
2015-01-01
CrystEngComm
Abstract:We report, for the first time, the ionic conductivity properties of two polymorphic structures of bismuth molybdates: Bi0.55MoO4 and Bi-2(MoO4)(3). A Bi0.55MoO4 single crystal was first synthesized, presenting a surprisingly high bismuth deficiency compared to the known stoichiometric phase Bi-2(MoO4)(3). It is expected to have a good oxide ion conduction due to the presence of Bi deficiency and oxygen vacancies. Bi0.55MoO4 crystallizes in the tetragonal system, space group I4(1)/a with a = b = 5.239(2), c = 11.567(5) angstrom, and Z = 4. While Bi-2(MoO4)(3) crystallizes in the monoclinic space group P2(1)/n, with unit cell parameters a = 7.71500(10), b = 11.5101(2), c = 11.1237(2) angstrom, beta = 103.3640(10)degrees, and Z = 4. Taking an advantage over many other ionic conductors, the crystals do not undergo any clear structural phase transition below their melting points. The oxide ion conductivities of Bi0.55MoO4 and Bi-2(MoO4)(3) were measured to be 6.5 x 10(-5) S cm(-1) and 1.1 x 10(-6) S cm(-1) at a temperature of 400 degrees C, respectively.
What problem does this paper attempt to address?