TIME-DEPENDENT DYNAMIC MODULUS PERCOLATION OF MULTI-WALLED CARBON NANOTUBES FILLED POLYSTYRENE MELTS DURING ANNEALING

Ai-zhi Guan,Yi-hu Song,Ye-qiang Tan,Qiang Zheng
DOI: https://doi.org/10.3724/sp.j.1105.2013.12111
2013-01-01
Acta Polymerica Sinica
Abstract:A study on rheological behavior of multi-walled carbon nanotubes (MWCNTs) filled polystyrene ( PS) melts submitted to isothermal annealing at temperatures from 170 degrees C to 190 degrees C was carried out. It is found that the filled PS melts with different volume fractions (phi) of MWCNTs from 0 to 0.05 underwent dynamic modulus percolation (DMP) during isothermal annealing and the DMP behaviors followed time-temperature superposition (TTS) principle disclosed for the first time. The filled melts with phi below percolation threshold exhibited liquid-like visco elasticity during annealing, and the activation energies (E-G' and E-G '') of the dynamic storage modulus (G') and loss modulus (G '') were higher and lower than that of viscous flow (E-w) of pure PS melt, respectively, but were in agreement with the dynamic modulus activation energies of dynamic moduli of PS melt at the same frequency as that used in DMP test, the dynamic moduli were obtained through the dynamic frequency experiment. Annealing the melts having phi above percolation threshold caused MWCNTs to aggregate further so much as that the melts changed from the liquid-like to the solid-like. In this case, both E-G' and E-Gn were smaller than E-w while energies (E-t' and E-tn) of liquid-like to solid-like transition were significantly higher than E-w. Moreover, the activation energies of dynamic modulus exhibited a sharp decrease in the percolation transition region. It was suggested that the isothermal time-dependent DMP was closely related to the formation of the MWCNTs aggregation-induced construction of three-dimensional elastic network while the terminal relaxation of PS macromolecules was not the determinant factor for DMP.
What problem does this paper attempt to address?