Phase separation strategy to facilely form fluorescent [Ag 2 ] 2+ /[Ag m ] n+ quantum clusters in boro-alumino-silicate multiphase glasses.
Xiaotong Chen,Junjie Zhao,Xiuxia Xu,Kai Ren,Xue Luo,Xinwen Sun,Xvsheng Qiao,Xianping Fan,Guodong Qian,Gaorong Han
DOI: https://doi.org/10.1039/c8cp04536d
IF: 3.3
2018-01-01
Physical Chemistry Chemical Physics
Abstract:By adjusting the content of ZnF2-SrF2/ZnO-SrO, a series of SiO2-Al2O3-B2O3-Na2O-ZnO/ZnF2-SrO/SrF2-Ag multiphase glasses was designed and prepared via a melt-quenching method. Under a phase separation strategy, negatively charged tetrahedrons ([BO4](-), [ZnO4](2-), and [AlO4](-)) can be generated to stabilize different silver species (Ag+ ions; [Ag-2](2+) pairs; [Ag-m](n+) quantum clusters ([Ag-m](n+) QCs)) in B2O3-rich and ZnO-Al2O3 rich sub-phases. The B2O3-rich sub-phase has a high solubility for Ag+ ions and [Ag-m](n+) QCs. The fluoride-rich phase shows a good ability to extract Na+ from the B2O3-rich sub-phase, significantly affects the solubility of Ag+ in the B2O3-rich sub-phase, and eventually determines the aggregation from Ag+ ions and Ag-0 atom to [Ag-m](n+) QCs. The ZnO-Al2O3-rich or ZnO-SiO2-rich (i.e. SiO2-rich in GZnOSrO) phase has a relatively high solubility for [Ag-2](2+) pairs. The Ag+/[Ag-2](2+)/[Ag-m](n+) QC fluorescent centers were identified by spectroscopic analysis, where the fluorescence bands are located in the ultraviolet, green-white and orange spectral regions, respectively. The fluorescent quantum yield (QY) of the [Ag-m](n+) QCs can be improved to 55.7%, and the combination of these three luminescent centers can achieve white light emission.