Abstract:Palladium/kieselguhr (Pd/K) composite with Pd of 45.3% was prepared by dipping-thermo decomposition with Pd(acac)2 as the precursor. Its hydrogenation/dehydrogenation cycles and anti-pulverization were studied by cool-heat cycles, PCT, XRD and SEM. The results of hydrogenation/dehydrogenation cycles showed that Pd/K composite were basically saturated in 30 s at 40°C, and its maximum hydrogen storage was 0.689%(mass fraction). Pd/K composite with initial particle size of 250~380 μm had stable hydrogen storage capacity, plateau and kinetics during 2000 cycles under the condition of hydrogenation at 40°C and dehydrogenation at 180°C, but the particle size less than 150 μm reached to 17.6%. The analysis of XRD and SEM indicated that Pd/K composite consisted of Pd and SiO2. Pd/K composite had higher content of Pd of surface of its particles. After heat treatment, the congregation of small particles of Pd carried out to form the film with porous micrograph. However, there were some cracks in the Pd film. As a result, Pd film easily detached from Pd/K composite particles during hydrogenation/dehydrogenation cycles. The high pulverization of Pd/K during the cycles was attributed to that the Pd was peeled from the surface of kieselguhr because of volume expansion.
What problem does this paper attempt to address?