Effect of γ-Al2O3 Pore Structure on Activity of Supported Pd Catalysts in C9 Petroleum Resin Hydrogenation
Jia Lu,Lei Ma,Dahao Jiang,Chunshan Lu,Qunfeng Zhang,Xiaonian Li
2011-01-01
Abstract:Three industrial γ-Al2O3s,namely W203,W217 and W251,were used as supports of Pd/γ-Al2O3 catalysts,in which W203 and W217 were typical mesoporous γ-Al2O3 supports,and W251 was a special macroporous support.Catalytic activity of the Pd/γ-Al2O3 catalysts in hydrogenation of C9 petroleum resin was investigated.The γ-Al2O3 supports and the Pd/γ-Al2O3 catalysts were characterized by means of N2 adsorption-desorption,CO chemisorption,SEM,TEM and XRD.The results indicated that the influence of the pore structure of the supported catalysts on the catalytic hydrogenation of C9 petroleum resin was significant and the catalyst with adequate macroporous structure showed higher activity and stability in catalytic hydrogenation of the macromolecules.Average pore sizes of the three industrial γ-Al2O3s,and activity and stability of the Pd/γ-Al2O3 catalysts followed with the same order: W203<W217<W251.Pd precursor could easily enter into W251 support interior with macropores,so the Pd dispersion was promoted and the catalyst with "egg white" structure formed.
What problem does this paper attempt to address?