Growth of Bulk Copper Single Crystal by Czochralski Technique

You-xin LOU,Ji-yang WANG,Huai-jin ZHANG,Qiang LI
DOI: https://doi.org/10.3969/j.issn.1000-985X.2011.03.005
2011-01-01
Abstract:The bulk (111) Cu single crystal with size of 12-19 mm ×85 mm was grown by Czochralski technique. The crystal structure and growth defect of as-grown crystal was investigated by XRD and optical microscope, and the resistivity was measured by Two-arm bridge method. The results demonstrated that the as-grown single crystal had a (111) crystalline orientation. The typical triangle etch pits were observed and its dislocation density was about 105-106 cm-2. The resistivity of (111) Cu single crystal was 1.289×10-8 Ω·m at room temperature.