Abstract:High silicon steel containing 6.5 wt% Si was prepared by pulse electrodepositon in KCl-NaCl-NaF-SiO2molten salt followed by diffusion annealing. The composition, the phase and the evolution of texture during the different production step were analyzed by glow discharge optical emission spectroscopy (GDOES), X-ray diffraction analysis (XRD) and the orientation distribution function (ODF). The results showed that the silicon content of the high silicon steel was about 6.5wt%. The high silicon steel was composed of a-Fe and Fe3Si. After diffusion annealing the undesirable g-fibre type texture {111} <110> and {111} <112> weakened, both easy magnetization direction Goss texture ({110} <001>) and cube texture {100} <001> were intensified.