Abstract:Polyethylene terephthalate (PET) fibers containing different contents of beta-nucleating agent (beta-NA) were meltspun from a reconstructive melt flow index rheometer at 270 degrees C, and then blended with polypropylene (iPP). The supermolecular and phase structure of the composite were investigated by polarized optical microscopy (POM), differential scanning calorimetry (DSC), and wide-angle X-ray diffraction (WAXD). For the pure PET fiber reinforced iPP, the interfacial region was mainly composed of alpha-modification, though it has been demonstrated that PET fiber shows weak nucleating ability towards iPP matrix. More interestingly, when the amount of beta-NA introduced into the PET fiber exceeds a critical value, the transcrystalline layer will be notably dominated by beta-modification. This method to prepare beta-transcrystallinity is remarkably different from those through stress or temperature control. The present results provide a facile and promising technique to prepare rich beta-transcrystallinity under stress-free conditions.
What problem does this paper attempt to address?