Ferroelectric-Relaxor Behavior of 0.8Batio3-0.2(Na1/4bi3/4)(mg1/4ti3/4)o3 Ceramic

Liying Wu,Xiaoli Wang,Jimmy H. Wang,Ruyan Guo,Amar S. Bhalla
DOI: https://doi.org/10.1080/07315170902938121
2009-01-01
Ferroelectrics Letters Section
Abstract:An onset of ferroelectric-relaxor like behavior of 0.8BT-0.2NBMT ceramics is studied in the temperature range from 15K to 573K. A broad dielectric peak with relatively high dielectric maximum shows frequency dispersion. The dielectric constant follows the modified Curie-Weiss law with the = 1.65. The relaxation rate follows the Vogel-Fulcher relaxation with E = 0.496 eV and TVF = 104.43K. The polarization hysteresis loops are observed with a small remnant polarization of 2.5 C/cm2 at room temperature.