Effect of 2–6 At.% Mo Addition on Microstructural Evolution of Ti-44Al Alloy
S. Z. Zhang,Z. W. Song,J. C. Han,C. J. Zhang,P. Lin,D. D. Zhu,F. T. Kong,Y. Y. Chen
DOI: https://doi.org/10.1016/j.jmst.2017.10.012
2018-01-01
Journal of Material Science and Technology
Abstract:In order to understand the effect of Mo alloying on the microstructural evolution of TiAl alloy, the as-cast microstructure, heat treated microstructure characteristic, and hot compression microstructure evolution of Ti-44Al alloy have been studied in this work. The as-cast microstructure morphology changes from (γ+α2) lamellar colony and β/β0+γ mixture structure to β/β0 phase matrix widmannstatten structure, when Mo content increases from 2 at.% to 6 at.%. Affected by the relationship between β phase and α phase, the angles between the lamellar orientation and the block β/β0 phase are roughly at 0°, 45° and 90°. Comparing with heat treatment microstructure, the hot compression microstructure contains less β/β0 phase, however, the β/β0 phase containing 2Mo alloy and 3Mo alloy hot compressed at 1275°C has the inverse tendency. In addition, (α2+γ) colony is decomposed by the discontinuous transformation.