Effect of tempering temperature on stress-corrosion cracking and mechanical hysteresis of 2Cr13 stainless steel

Xiang-qun ZHU,Qi-xun DAI,Ming ZHOU,De-jun KONG
2009-01-01
Abstract:The stress-corrosion cracking (SCC) characteristics of 2Cr13 stainless steel quenched from 1020°C and tempered at different temperatures were tested by slow strain rate test (SSRT) method. Meanwhile, the strain gage based load cell technique was employed to investigate the mechanical hysteresis of 2Cr13 stainless steel after tempering. The result shows that from 270 to 420°C, with increasing tempering temperature, the strength and mechanical hysteresis of 2Cr13 stainless steel slightly increases and reduces, respectively, along with a substantial increase of the susceptibility of SCC. It indicates that in the range of 270 to 420°C, with increasing tempering temperature, which is closer to the sensitization and tempering embrittleness temperature of 2Cr13 stainless steels, added to secondary hardening effect, by which the resistance of SCC of 2Cr13 stainless steel considerably decreases with increasing tempering temperature. Mechanical hysteresis of 2Cr13 stainless steel is related to the microstructure and strength, hysteresis error decreases with increasing materials strength.
What problem does this paper attempt to address?