Sm2O3 and MnO2 codoped PMN-PZT ceramics with both high mechanical quality factor and piezoelectric properties
Chao Wang,Li Ning,Qi Li,Yang Li,Xinya Feng,Mingwen Wang,Xuechen Liu,Shuai Yang,Jie Wu,Jinglei Li,Fei Li
DOI: https://doi.org/10.1016/j.ceramint.2023.03.246
IF: 5.532
2023-03-01
Ceramics International
Abstract:For lead-based ceramics used in high-power devices, it is essential that they possess both a high mechanical quality factor (Q m) and a large piezoelectric coefficient (d 33). Unfortunately, Q m is inversely proportional to d 33 for piezoelectric ceramics, which the limits their actual application. If suitable acceptor and donor dopants can be added in piezoelectric ceramics, it is rational to achieve high Q m and large d 33 simultaneously. Herein, we tried to achieve both a high mechanical quality factor and large piezoelectric activity in 0.47 pb(Mg1/2Nb2/3)O3-0.18PbZrO3-0.35PbTiO3 (PMN-PZT) ceramics via Sm2O3 and MnO2 co-doing. A range of xMn-2Sm-PMN-PZT ceramics were fabricated by the traditional sintering method. An optimal performance was attained in 4Mn-2Sm-PMN-PZT ceramics with Q m = 1720, d 33 = 450 pC/N, ε = 2720 and k p = 0.54. The high Q m is related to the presence of defect dipoles as a result of MnO2 doping and the large piezoelectric activity is due to the doping of Sm2O3.
materials science, ceramics